8. Preheat Settings 预热设置
Note:the printing preheating parameter standard has been adjusted when leaving the factory. PLA preheating standard: nozzle temperature 200°C,Hot bed
temperature 60°C, ABS preheating standard: nozzle temperature 240°C, hot bed temperature 70°C.
If it needs to be adjusted for printing materials or other reasons, you can temperature → on the front page of the interface PLA/ABS preheating setting for parameter
adjustment adjustment.
注意:打印预热参数标准出厂时已调整好,PLA预热标准:喷嘴温度200°C,热床温度60°C,ABS预热标准:喷嘴温度240°C,热床温度70°C。
若因打印材料或其他原因需要调整,可以在界面首页温度→PLA/ABS预热设置进行参数调整。
EN
CN
17
    "